1.Check the operating welding machine and the temperature should be up to 260 ℃ .2.Mark PPR pipe the access depth before welding(25mm depth is about 1.5cm)3.Parallel the pipe and fitting into the welding head for 4 seconds' duration 4.Pulling out the pipe and fittings after fully heated and keeping