SAM-UK builds this PVC water supply single union ball valve with one union nut and one
fixed end — the union side is the service side, so the end connector comes off without cutting pipe.
It will not lift the whole body out of a line; that is a double union, and we make those
too. Socket or BSPP threaded ends, PN16 body, TPV seats, EPDM O-rings, ABS wing handle.
OEM marking available.

Construction pipeline system
Agricultural irrigation pipeline system
Pool pipeline system
Industrial pipeline system
Water treatment pipeline system
Fishery aquaculture pipeline system
The characteristics of PVC material: stable physical properties, and not suitable for acid and alkali corrosion, relatively heat-resistant. By adding different additives, PVC materials can present different physical and mechanical properties
| Benefits |
| Long service life |
Electrical insulation |
Good impact elasticity |
Good chemical resistance |
Easy to operate |
light in weight |
A single union valve has one nut and one fixed end. The union side is the service side: undo the nut
and the end connector comes off the body — no saw, no drained line, no cutting. What it will not
do is lift the whole valve out of the pipe. That is a double union, a different casting — we make it
too. Pull a body out of a live manifold and you want the double union; change an end,
align a thread or replace a cracked connector and this is the cheaper way.
That last point is the one buyers underrate. The end connector is a separate moulded
part, so a socket valve can become a threaded valve by swapping one piece instead of
scrapping the whole body. Distributors who stock both end types stop tying up capital in two
complete SKUs.
Six parts, four materials, and only one of them sets the temperature limit. Body, ball,
stem, end connector, flange and union nut are PVC — the whole wetted path is one material.
Seats are TPV, O-rings are EPDM, the handle is ABS.
The union nut’s O-ring is a compression seal, not a gasket. It seals because it
sits in a groove under squeeze; crank the nut down hard enough and the ring deforms permanently, then
weeps — not at commissioning, but a season later. Hand-tight plus a snug quarter turn is the whole
specification.
The 60 °C ceiling comes from the PVC, not the seals — TPV and EPDM both run far
hotter in service. That is why the temperature figure sits beside the pressure figure, not in a
materials list.
The body takes either end pattern; the difference is how that end meets the pipe.
Socket (solvent weld). Permanent, cheapest per joint, and the strongest joint in
the system when done properly — primer, cement, a square-cut dry end, the full cure window. It never
comes apart: fine on new build, miserable on a retrofit.
Threaded. Removable, and the right choice wherever the valve has to come off for
inspection. Two things kill threaded PVC joints: solvent cement, which should never touch a thread,
and over-tightening. A PVC male thread will crack before it stops turning, and the crack
shows up weeks later as a weep — long after the installer has left site.
The thread form is the other trap. BSPP (ISO 228-1, G thread) is parallel, not tapered,
and it is not interchangeable with NPT. NPT seals on the thread flanks; BSPP needs a face
seal or an O-ring. Mate the two and you get a joint that holds at low pressure and weeps at test
pressure — the worst possible timing. We mould to G1/2, G3/4 and G1; check it against the pipe before
the order, not after.
Three sizes, one water-supply body. Socket and threaded versions share the same body — only
the end connector changes, so a mixed order is one valve design and one spare-parts list.
| Size | I | L1 | L2 | d1 | d2 | D1 | D2 | H |
|---|---|---|---|---|---|---|---|---|
| 20 (1/2″) | 17.5 | 79.5 | 75.6 | 21.54 | 15.0 | 50.0 | 29.0 | 59.5 |
| 25 (3/4″) | 18.3 | 89.6 | 80.0 | 26.87 | 20.0 | 60.7 | 34.0 | 66.2 |
| 32 (1″) | 22.3 | 101.0 | 90.0 | 33.65 | 24.4 | 68.0 | 42.0 | 76.6 |
Threaded ends are BSPP: G1/2, G3/4 and G1 against the three sizes. Dimension symbols
are marked on the line drawing at the top of this page.
Pressure rating: PN16 (16 bar, 232 psi), quoted on water at 20 °C. Service
temperature runs to 60 °C maximum, and PVC loses allowable pressure as the line
warms — at 60 °C this body carries roughly half its cold rating, around 8 bar. A
pressure figure without a temperature attached is not a rating, it is a guess, which is why both
belong in the same sentence.
This model is CE marked and moulded under an ISO 9001 system. Those are the two
documents we can put in your inbox today.
It does not carry NSF/ANSI 14 or UPC listing. If the job needs potable-water
listing for the US or Canada, say so before the order — that is a different product with a
different test file, not a certificate we can print afterwards. Every claim on this page is
limited to what the listing actually covers, and on this valve that limit is CE plus ISO
9001.
Four failures account for nearly every return:
Taizhou Zhuoxin Plastics has been moulding pipe and fittings since 1995 — 300 to
350 staff, 50,000 tonnes a year, and a mould shop on the same site as the injection
lines. That is why a non-standard end configuration or a private-label marking is a drawing revision
rather than a tooling programme. Valve bodies and union nuts come off our own moulds, so the seal
face and the nut that loads it are matched by design, not by tolerance stacking.
Fittings, valves and pipe ship on one set of documents, in one container, on a
30-45 lead time. For a distributor building a mixed order, that usually
beats a few points on unit price.
Single union: the body stays on the pipe, only the end connector comes off. Double union: both
ends have nuts, so the whole valve lifts out. If a failed body has to come out of a live line,
you need the double union. If you are changing an end type or replacing a cracked connector, the
single union does it with one nut and no cutting.
No — and be careful with suppliers who say you can. On this valve only the union-end connector
comes off; the fixed end is welded or threaded into the run. For full body removal, order the
double union version.
No. Isolation only. Throttling a part-open ball erodes the seat, and PVC is not built to absorb
that.
Water, most acids and alkalis are fine. Solvents, aromatics and chlorinated hydrocarbons —
acetone, toluene and their relatives — are not. EPDM also swells on mineral oil, which rules out
a lot of compressor and hydraulic lines. Check the media against a chemical resistance table
before the order, not after.
① Pipe cutting: according to the use requirements, after measuring the appropriate length, the required pipe can be cut by hand or machine. When cutting, keep both ends vertical and flat, and use a file to cut Deburring and sharp edge, but the chamfer should not be too large.
② Bonding of pipes and fittings: before bonding, trial assembly must be carried out, installation position must be determined and marked, length of inserted pipe end (socket depth + 10mm) and inner wall of socket of pipe fittings shall be cleaned,Then wipe with cotton yarn stained with acetone. After acetone volatilizes, evenly brush the adhesive on the outside of pipe end and inside of socket. It should not be too thick, but it should not be missed. Insert after painting and rotate. To the ideal combination angle required for installation, make all the pipes inserted into the socket, fix them by themselves after about 2 to 3 minutes, and wipe off the excess adhesive overflowing from the bonding place to keep the pipe clean. Now cut.Do not force to open or rotate the direction, otherwise it will cause leakage. The adhesive component shall not be subjected to external force within 1 hour, and shall not be watered within 24 hours. The test can be conducted only after the curing time is completed.
③ The pipeline installation must have a reliable seal to ensure that there is no leakage in the process of use. Fixing devices (pipe clamps) shall be installed every 1.5m to 2.0m.
④ Because the plastic pipe has certain plasticity, when the horizontal pipe is installed, the bracket or elevator is set every 0.6m to prevent the plastic pipe from deformation and affect the use.
⑤ The water supply pipe shall be far away from the heat source, and the clear distance between the riser and the stove edge shall not be less than 400mm, and the clear distance between the riser and the heating pipe shall not be less than 200mm.
⑥ After construction, the pipe can be sealed with soil only after passing the pressure test.
⑦ Please refer to the relevant construction specifications of the Ministry of construction for specific installation and use.